Drinking water transfer printing films consist of a clear layer of polyvinyl liquor (PVA), that's printed with a range of decorations. The ink layer is then sealed. The PVA layer dissolves on speak to with water. Thereafter, the seal is dissolved by an activator (a special type of solvent) and only the shade layer stays. The paint layer adheres for the workpiece immersed and behaves similar to a lacquer layer right after drying.
The best h2o temperature to the process of printing h2o movies is 32 ° C. In chilly climate up to 34 ° Celsius.
The transfer h2o transfer film should be lower on all sides at a length of one cm to stop winding when placing within the area on the h2o. Make sure you do not stay with tape due to the fact the film can't rise in the course of the immersion process (In case the PVA is dissolved, the film "relaxes" as well as the area measurement will increase minimally).
After the desired publicity time, spray the movie at a distance of 20-30 cm in the direction of crossover with activator of twenty five to forty five g / m² (depending on the reason, given that extremely printed films want much more activator).
The workpiece may be immersed soon after approx. fifteen seconds.
All components that are not made from Abdominal muscles plastic should be geared up before diving (eg by lacquering).
Right after approx. One particular moment, the workpiece must be washed with hot h2o at 42 ° C (tend not to make use of a sturdy h2o jet, portions of the movie could dissolve).
The coloration proven may differ from the first film according to the output unit. For a consequence that is corresponding to the picture, the colour suggestion background must match the chosen water transfer print movie.
The best h2o temperature to the process of printing h2o movies is 32 ° C. In chilly climate up to 34 ° Celsius.
The transfer h2o transfer film should be lower on all sides at a length of one cm to stop winding when placing within the area on the h2o. Make sure you do not stay with tape due to the fact the film can't rise in the course of the immersion process (In case the PVA is dissolved, the film "relaxes" as well as the area measurement will increase minimally).
After the desired publicity time, spray the movie at a distance of 20-30 cm in the direction of crossover with activator of twenty five to forty five g / m² (depending on the reason, given that extremely printed films want much more activator).
The workpiece may be immersed soon after approx. fifteen seconds.
All components that are not made from Abdominal muscles plastic should be geared up before diving (eg by lacquering).
Right after approx. One particular moment, the workpiece must be washed with hot h2o at 42 ° C (tend not to make use of a sturdy h2o jet, portions of the movie could dissolve).
The coloration proven may differ from the first film according to the output unit. For a consequence that is corresponding to the picture, the colour suggestion background must match the chosen water transfer print movie.
Examine out this website: http://cursopinturahidrografica-wtp.com